production Extruded tube It will burst for a long time due to frequent and severe pressure shocks. This situation is usually not caused by excessive static pressure, but is related to the strength and frequency of pressure shock. During the operation of construction machinery, the oil pressure in the oil resistant hose will rise or fall repeatedly, and then it will form frequent pressure shocks to the oil pipe, causing the oil seal of each part to become more damaged, the oil resistant hose will bubble and break, and the pipe joint will become loose and leak. Therefore, in the process of operation, the valve rod should not be pulled too hard, and it needs to be gentle. The application temperature of the oil in the oil resistant rubber hose is too high, resulting in aging and bursting of the rubber hose. During the operation of construction machinery, the hydraulic system will cause the oil to become hot due to power failure, and the influence of external temperature (especially in summer) will cause the oil temperature to rise sharply. The higher the oiling temperature is, the easier the rubber hose ages, the worse the elasticity is, the lower the strength and sealing function are, and the oil resistant hose will burst quickly. Therefore, Extruded tube company During operation, when the temperature rise of the hydraulic system is too high or too fast, the causes should be found and eliminated in time. Necessary cooling measures shall be taken for summer operation, especially continuous operation.
Shandong Extruded tube It is composed of sand blasting hose, net sleeve and joint. The sand blasting hose is the main body of the rubber sand blasting pipe, playing a flexible role, and the net plays a role of strengthening and shielding; Joints play the role of connection. For different use requirements, they are connected in different ways: sandblasting hose, net sleeve and joint are connected by welding, which is called welding type; The connection in the form of mechanical clamping is called mechanical clamping. In addition, the combination of the above two methods is called hybrid clamping. Rubber sand blasting pipe products include oil suction hose, steam hose, sand blasting hose, acid and alkali suction hose, food hose, oxygen blowing hose and various special-shaped hoses. It is widely used in machinery, chemical industry, petroleum, metallurgy, food and other industries. What is the pressure range of pressure resistant rubber sand blasting pipe: the pressure range of hose is generally Pn 0.6-32.0 MPa. The rubber sand blasting pipe up to 42.0 MPa is the main pressure bearing part of the hose installed in the pressure pipe, and it acts as the sheath of the sand blasting hose. Extruded tube company One or more layers of stainless steel wire or steel strip can be selected for braiding according to the pressure in the pipeline and the place of use. It can also achieve the effect of reducing noise. This is why some rubber sand blasting pipes use rubber sand blasting pipes.
production Extruded tube 1. During the molding of rubber products, the cohesive force of the elastomer cannot be eliminated due to the large pressure pressing. During the molding and mold release, extremely unstable shrinkage (the shrinkage rate of rubber varies due to different rubber types) often occurs. It must take a period of time before it can be gentle and stable. Therefore, at the beginning of the design of a rubber product, no matter the formula or the mold, it is necessary to carefully calculate the matching. If not, it is easy to cause dimensional instability of the product, resulting in low product quality. 2. Rubber belongs to thermosetting elastomer, while plastic belongs to thermosetting elastomer. Due to different sulfide types, the temperature range of rubber molding and curing is quite different, even affected by climate change and indoor temperature and humidity. Therefore, the production conditions of rubber products need to be properly adjusted at any time. If not, there may be differences in product quality. 3. The rubber product is the rubber mixture made from rubber raw materials after mixing in the internal mixer as the raw material. The formula is designed according to the characteristics of the required rubber products during mixing, and the required product hardness is determined. The product is molded by the rubber plate vulcanizer. After the product is formed, flash processing shall be carried out to make the product surface smooth without burrs. 4. The aging test of rubber products belongs to the category of aging test. Rubber aging refers to the phenomenon that the performance and structure of rubber and products are changed due to the combined effect of internal and external factors in the process of processing, storage and use, thus losing their use value. Extruded tube company It is characterized by cracking, tackiness, hardening, softening, chalking, discoloration, mildew, etc. The following conditions shall be met when the ball mill uses the rubber lining plate: 1. The hardness of the ground material. The iron base alloy is similar to the rubber lining plate for materials below medium hardness, and the rubber lining plate is superior for materials above medium hardness. 2. The temperature of rubber lining plate is generally 70 ℃ - 90 ℃, and it can reach 110-130 ℃ under special circumstances. The temperature should be lower during dry grinding. 3. Feed size. Generally, the ball mill shall be more than 20-25mm; For the autogenous mill, the feeding particle size can be larger because no steel ball is added.
Whether in the process of purchase or use, production Extruded tube The quality of all needs to be checked regularly. During the inspection, the following items should be noted. 1. Standard size and actual error of high-pressure rubber hose: because the inner diameter and outer diameter of high-pressure sand blasting pipe and the outer diameter of the skeleton layer will shake, if the shaking amplitude exceeds the allowable limit, the balance of the buckling amount of the sand blasting pipe joint cannot be guaranteed, and the quality of the sand blasting pipe assembly cannot be guaranteed. Therefore, for the sand blasting pipe selected for the production of sand blasting pipe assembly, it is necessary to strictly check whether the inner diameter and outer diameter of the skeleton layer meet the requirements, and the requirements for the outer diameter error can be appropriately relaxed. 2. Wall thickness error of high-pressure hose: due to the local pain of the rubber layer in the high-pressure sandblasting pipe and the influence of the overlapping width of the rubber layer in the high-pressure sandblasting pipe quality inspection center between the skeleton layers, the wall thickness error of the sandblasting pipe may be too large. If the wall thickness error exceeds the allowable range, it will affect the tightness and pull-out strength of the connector, and even cause some deflection (tilting head) of the hose assembly connector. Quality inspection of high-pressure sand blasting pipe Therefore, the wall thickness error of sand blasting pipe should be strictly controlled. Generally, the rubber hose with wall thickness error exceeding 0.5mm shall be selected stably. 3. Adhesion between each layer of high-pressure rubber hose: high-quality high-pressure sand blasting pipe shall have prominent integrity, that is, the quality inspection of high-pressure sand blasting pipe shall have high adhesion between each structural layer, and the adhesion between each adhesive layer shall become an integrity. Only in this way can we meet various technical requirements in the process of joint installation and fastening, and only in this way can we ensure the quality inspection requirements of high-pressure sand blasting pipes for sand blasting pipe assembly. Therefore, Extruded tube company It is necessary to control the adhesive force between each layer of the rubber hose not lower than that specified in the technical standard, and the rubber hose with high adhesive force shall be selected as far as possible to produce the rubber hose assembly.
Shandong Extruded tube There are many specifications. Different installation positions require different specifications of cloth clamping sand blasting pipe, and the specification selection of cloth clamping sand blasting pipe has different requirements. The following small series will briefly introduce them to you: 1. Temperature: The selection should be based on the ambient temperature when the cloth clip sandblasting pipe is working. In case of high temperature, the temperature correction pressure shall be determined according to the working pressure and temperature correction coefficient of the cloth sanding pipe under high temperature to determine the correct pressure level. 2. Pressure: when selecting the cloth clip sandblasting pipe, check the nominal diameter and pressure gauge of the corrugated cloth clip sandblasting pipe according to the actual working pressure of the hose to determine whether to use the stainless steel mesh sleeve type. 3. Size: select the joint type, size of cloth sanding pipe and hose length according to the size of cloth sanding pipe. 4. Medium: determine the material of each part of the hose according to the chemical properties of the material medium transported in the cloth sanding pipe and the corrosion resistance of the hose material. 5. Status: According to the use status of the hose, refer to the correct use and installation method of the cloth clip sandblasting pipe and the length of the hose in the settlement compensation. Therefore, Extruded tube company According to the actual pressure of the system, the higher the working pressure of the cloth clamping sand blasting pipe is, the normal operation of the system can be ensured, and the appropriate cloth clamping sand blasting pipe is selected.
Extruded tube company It has become the standard configuration of the modern new ball mill, but many problems may occur during the use or installation of the rubber lining plate, which will cause the failure of the rubber lining plate of the ball mill. Here is a brief introduction to the causes of the more common failure of the rubber lining plate of the ball mill. The design and installation are not professional and reasonable. The design and installation are also common problems for many novice manufacturers. For example, the bolt holes for fixing the ball mill lining plate are square, which will cause stress concentration and fracture. Adjust the size of lining plate to control the gap between lining plates at about 8mm; The installation quality of lining plate is very important to the safe operation of ball mill. First, tighten the fixed wedge symmetrically, put the lining plate in sequence, and then use the tightening wedge to secure it; Therefore, professional installation guidance can easily avoid these problems. The reason why the rubber lining plate of the ball mill does not match the steel ball is relatively common, and it is easy for many novice manufacturers to ignore and make mistakes. During the operation of the ball mill, the rubber lining plate of the ball mill, materials and steel balls promote the normal grinding and crushing of the ball mill due to the interaction of forces. The hardness of materials is related to wear resistance, and the wear resistance increases with the increase of hardness, Shandong Extruded tube It is a pair of friction pairs, and the increase of hardness of one side will cause the wear of the other side to increase. Therefore, the high wear-resistant rubber lining plate is matched with the high wear-resistant steel ball, and the low wear-resistant rubber lining plate is matched with the low wear-resistant steel ball, so as to ensure the normal wear of the rubber lining plate of the ball mill and extend the service life of the ball mill.